| Project No. | EN 1252-2:2001 |
|---|---|
| Title | This European Standard specifies the toughness requirements of the metallic materials for use at a temperature between - 80 °C and - 20 °C ensuring suitability for use for the cryogenic vessels. Fine grain and low alloyed steels with specified yield strength <= 460 N/mm², aluminium and aluminium alloys, copper and copper alloys and austenitic stainless steels are covered by this standard. |
| Registration number (WIID) | 13654 |
| Scope | This European Standard specifies the toughness requirements of the metallic materials for use at a temperature between - 80 °C and - 20 °C ensuring suitability for use for the cryogenic vessels. Fine grain and low alloyed steels with specified yield strength <= 460 N/mm², aluminium and aluminium alloys, copper and copper alloys and austenitic stainless steels are covered by this standard. |