ASD-STAN
| Project No. | prEN 3873 |
|---|---|
| Title | This document specifies the requirements for determining fatigue crack growth rates using corner-crack (CC) test pieces. Crack development is measured using a potential-drop system, and the calculated crack depths can be corrected via marker bands created on the fracture surface during the test. Results are expressed in terms of the crack-tip stress-intensity range (ΔK), with crack depths and test stress level noted. |
| Registration number (WIID) | 72606 |
| Scope | This document specifies the requirements for determining fatigue crack growth rates using corner-crack (CC) test pieces. Crack development is measured using a potential-drop system, and the calculated crack depths can be corrected via marker bands created on the fracture surface during the test. Results are expressed in terms of the crack-tip stress-intensity range (ΔK), with crack depths and test stress level noted. |
| Status | Aptauja |
| ICS group | 49.025.15 49.025.05 |