Project No.ISO 2039-1:1993
Title<p>Specifies a method, which consists of forcing a ball under a specified load into the surface of a test specimen. The depth of impression is measured under load. The surface area of the impression is computed from its depth. The ball indentation hardness is then calculated from the following relationship: Ball indentation hardness = Applied load : Surface area of impression.</p>
Registration number (WIID)21467
Scope<p>Specifies a method, which consists of forcing a ball under a specified load into the surface of a test specimen. The depth of impression is measured under load. The surface area of the impression is computed from its depth. The ball indentation hardness is then calculated from the following relationship: Ball indentation hardness = Applied load : Surface area of impression.</p>
StatusAtcelts
ICS group83.080.01