ASD-STAN
Registration number (WIID) | Project No. | Title | Status |
---|---|---|---|
30926 | prEN 3475-811 | Aerospace series - Cables, electrical, aircraft use - Test methods - Part 811: Unbalance attenuation | Izstrādē |
76917 | prEN 3475-811 | Aerospace series - Cables, electrical, aircraft use - Test methods - Part 811: Unbalance attenuation | Aptauja slēgta |
81186 | prEN 3475-812 | Aerospace series - Cables, electrical, aircraft use - Test methods - Part 812: Return loss (VSWR) | Aptauja |
17199 | prEN 3483 | Steel FE-CM61 - Homogenised, solution treated, precipitation hardened and sub zero - RM >or= 1240 MPa - High strength - Sand or investment casting | Izstrādē |
17201 | prEN 3485 | Steel FE-CM61 - Homogenised, solution treated, precipitation hardened and sub zero - RM >or= 830 MPa - Medium strength - Sand or investment casting | Izstrādē |
17208 | prEN 3492 | Steel FE-PM44 - Hardened and tempered - Bar for machining - DE <or= 150 mm | Izstrādē |
17209 | prEN 3493 | Steel FE-PL48 - Hardened and tempered - 1050 <or= RM <or= 1250 MPa - Forgings - DE <or= 40 mm | Izstrādē |
17210 | prEN 3494 | Titanium alloy TI-P11 - Solution treated and aged - 650 <or= RM <or= 880 MPa - Forgings - DE <or= 75 mm | Izstrādē |
17211 | prEN 3495 | Titanium alloy TI-P11 - Annealed - 540 <or= RM <or= 770 MPa - Forgings - DE <or= 150 mm | Izstrādē |
17212 | prEN 3496 | Titanium alloy TI-P04 - Annealed - 540 <or= RM <or= 740 MPa - Forgings - DE <or= 150 mm | Izstrādē |
Displaying 6731-6740 of 7068 results.