This European Standard specifies three test methods for determining the effect of saturation and accelerated water conditioning:
- method A uses the indirect tensile strength of cylindrical specimens of bituminous mixtures;
- method B uses the compression strength of cylindrical specimens of bituminous mixtures;
- method C defines the bonding value for a bituminous mixture 1 h after mixing, where the bonding of bitumen and aggregate can be equated to a bonding value.
Method C is suitable for soft asphalt with bitumen of kinematic viscosity at 60 °C of 4 000 mm2/s or less.
These methods can be used to evaluate the effect of water on asphalt mixtures with or without anti-stripping additives including liquids, such as amines; and fillers, such as hydrated lime or cement.
Reģistrācijas numurs (WIID)
80734
Darbības sfēra
This European Standard specifies three test methods for determining the effect of saturation and accelerated water conditioning:
- method A uses the indirect tensile strength of cylindrical specimens of bituminous mixtures;
- method B uses the compression strength of cylindrical specimens of bituminous mixtures;
- method C defines the bonding value for a bituminous mixture 1 h after mixing, where the bonding of bitumen and aggregate can be equated to a bonding value.
Method C is suitable for soft asphalt with bitumen of kinematic viscosity at 60 °C of 4 000 mm2/s or less.
These methods can be used to evaluate the effect of water on asphalt mixtures with or without anti-stripping additives including liquids, such as amines; and fillers, such as hydrated lime or cement.