<p>Defines the method as an interim method because the reproducibility between various laboratories is still too different. The crushing strength of individual pellets can affect the dispersion of carbon black in polymers, on bulk handling, and on conveying properties.</p>
Reģistrācijas numurs (WIID)
16466
Darbības sfēra
<p>Defines the method as an interim method because the reproducibility between various laboratories is still too different. The crushing strength of individual pellets can affect the dispersion of carbon black in polymers, on bulk handling, and on conveying properties.</p>