Informējam, ka Sistēma pielāgota darbam ar interneta pārlūkprogrammu Internet Explorer (8. un jaunākām versijām) un Mozilla Firefox (3.6 un jaunākām versijām).
Izmantojot citu interneta pārlūkprogrammu, brīdinām, ka Sistēmas funkcionalitāte var tikt traucēta.
<p>ISO 16507:2013 is applicable to determining the resistance to deflection and damage of wood-based panels subjected to concentrated impact loads from nonrigid blunt objects, concentrated static loads, and uniformly distributed loads. Surface indentation is not evaluated separately from deflection.</p>
<p>The procedures are intended to simulate loading on roof or floor sheathing materials installed directly to framing. Three applications are covered: roof sheathing, subfloors, and single floors. Panels are tested parallel and/or perpendicular to the panel strength axis. Roof sheathing is tested in both a dry and a wet condition, while subfloors and single floors are both tested in a dry condition, as well as a condition of having dried out after being wet. These moisture conditions are those commonly experienced with site-built construction.</p>
<p>These procedures do not cover vibration and are not intended for the evaluation of the framed assembly as a whole.</p>
Reģistrācijas numurs (WIID)
56899
Darbības sfēra
<p>ISO 16507:2013 is applicable to determining the resistance to deflection and damage of wood-based panels subjected to concentrated impact loads from nonrigid blunt objects, concentrated static loads, and uniformly distributed loads. Surface indentation is not evaluated separately from deflection.</p>
<p>The procedures are intended to simulate loading on roof or floor sheathing materials installed directly to framing. Three applications are covered: roof sheathing, subfloors, and single floors. Panels are tested parallel and/or perpendicular to the panel strength axis. Roof sheathing is tested in both a dry and a wet condition, while subfloors and single floors are both tested in a dry condition, as well as a condition of having dried out after being wet. These moisture conditions are those commonly experienced with site-built construction.</p>
<p>These procedures do not cover vibration and are not intended for the evaluation of the framed assembly as a whole.</p>