<p>Fire assaying comprises the following steps: crucible fusion, cupellation, parting (followed by flame atomic absorption spectrometry), retreatment, correction for blank contamination. The method is applicable for copper sulfide concentrates containing 15 % (m/m) to 60 % (m/m) copper, mainly in the form of chalcopyrite and related sulfide minerals, and gold contents from 0,5 g/t to 300 g/t and silver contents from 25 g/t to 1500 g/t.</p>
Reģistrācijas numurs (WIID)
18439
Darbības sfēra
<p>Fire assaying comprises the following steps: crucible fusion, cupellation, parting (followed by flame atomic absorption spectrometry), retreatment, correction for blank contamination. The method is applicable for copper sulfide concentrates containing 15 % (m/m) to 60 % (m/m) copper, mainly in the form of chalcopyrite and related sulfide minerals, and gold contents from 0,5 g/t to 300 g/t and silver contents from 25 g/t to 1500 g/t.</p>