<p>ISO 26443:2008 specifies a method for the qualitative evaluation of the adhesion of ceramic coatings up to 20 µm thick by indentation with a Rockwell diamond indenter. The formation of cracks after indentation may also reveal cohesive failure. The indentations are made with a Rockwell hardness test instrument.</p>
<p>The method described may also be suitable for evaluating the adhesion of metallic coatings.</p>
<p>The test is not suitable for elastic coatings on hard substrates.</p>
Reģistrācijas numurs (WIID)
43584
Darbības sfēra
<p>ISO 26443:2008 specifies a method for the qualitative evaluation of the adhesion of ceramic coatings up to 20 µm thick by indentation with a Rockwell diamond indenter. The formation of cracks after indentation may also reveal cohesive failure. The indentations are made with a Rockwell hardness test instrument.</p>
<p>The method described may also be suitable for evaluating the adhesion of metallic coatings.</p>
<p>The test is not suitable for elastic coatings on hard substrates.</p>