<p>ISO 17161:2014 describes a procedure to verify the degree of misalignment of the load train of the test machines using a reference test specimen uniformly loaded in tension or in compression, and to give indications in order to correct defects such as torsion and bending.</p>
<p>ISO 17161:2014 is not intended to provide a quantitative and acceptable limit before the testing of ceramic matrix composites with a fibre reinforcement: unidirectional (1D), bidirectional (2D), and tridirectional (<i>x</i>D, with 2 < <i>x</i> ≤ 3) loaded along one principal axis of reinforcement. This limit depends on the sensitivity of each type of composite to the misalignment defect.</p>
Reģistrācijas numurs (WIID)
59200
Darbības sfēra
<p>ISO 17161:2014 describes a procedure to verify the degree of misalignment of the load train of the test machines using a reference test specimen uniformly loaded in tension or in compression, and to give indications in order to correct defects such as torsion and bending.</p>
<p>ISO 17161:2014 is not intended to provide a quantitative and acceptable limit before the testing of ceramic matrix composites with a fibre reinforcement: unidirectional (1D), bidirectional (2D), and tridirectional (<i>x</i>D, with 2 < <i>x</i> ≤ 3) loaded along one principal axis of reinforcement. This limit depends on the sensitivity of each type of composite to the misalignment defect.</p>