<p>ISO 15733:2015 specifies the conditions for determination of tensile properties of ceramic matrix composite materials with continuous fibre reinforcement at room temperatures. This International Standard applies to all ceramic matrix composites with a continuous fibre reinforcement, unidirectional (1D), bi-directional (2D), and tri-directional (<i>x</i>D, with 2 < <i>x</i> ≤ 3), loaded along one principal axis of reinforcement.</p>
<p>NOTE In most cases, ceramic matrix composites to be used at high temperature in air are coated with an antioxidation coating.</p>
Reģistrācijas numurs (WIID)
62149
Darbības sfēra
<p>ISO 15733:2015 specifies the conditions for determination of tensile properties of ceramic matrix composite materials with continuous fibre reinforcement at room temperatures. This International Standard applies to all ceramic matrix composites with a continuous fibre reinforcement, unidirectional (1D), bi-directional (2D), and tri-directional (<i>x</i>D, with 2 < <i>x</i> ≤ 3), loaded along one principal axis of reinforcement.</p>